Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ecomass® 1700TU96 Tungsten Filled Polyamide

Category Polymer , Thermoplastic , Nylon
Manufacturer Ecomass Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 1700TU96 Tungsten Filled Polyamide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyRigidInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 11.0 g/cc
11.0 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0060 cm/cm
0.0050 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Tensile Modulus 9.65 GPa
1400 ksi
ASTM D638
Flexural Strength 63.4 MPa
9200 psi
ASTM D790
Flexural Modulus 8.41 GPa
1220 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 159 °C
318 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 155 °C
311 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.21 ohm
0.21 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 204 - 254 °C
400 - 490 °F
Mold Temperature 57.2 - 82.2 °C
135 - 180 °F
Drying Temperature 73.9 °C
165 °F
Dry Time 4 hour
4 hour