Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.14 GPa | 1180 ksi | ASTM D790 |
Omni Plastics OmniTech™ ABS GRC30 NA Glass Reinforced OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Flexural Modulus | 8.14 GPa | 1180 ksi | ASTM D790 |
Polymer Resources PPX/NY G30 PPO/Nylon 66 Alloy , 30% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Flexural Modulus | 8.14 GPa | 1180 ksi | (50.8 mm Span) 1mm/min; ASTM D790 |
LNP ULTEM® UCF1205 Polyetherimide, 12% Carbon Fiber Reinforcement, 5% PTFE Lubricant
(discontinued **) Office equipment internal parts.Features: Lubricated, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labe.. |
|||
Flexural Modulus | 8.14 GPa | 1180 ksi | ASTM D790 |
Samyang Tramid® 910 PA66/PA6 Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.Applications:Automotive knob types, door handles and mirror housingsConnectorsCab.. |
|||
Flexural Modulus | 8.14 GPa | 1180 ksi | ASTM D790 |
Techmer ES HiFill® PA6 0325 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityTPC# 6066102Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 8.14 GPa | 1180 ksi | ASTM Value |
BASF Capron® 8333G HI HS BK-102 Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8333G HI HS BK-102 is a 33% glass reinforced, impact modified polyamide 6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughness in c.. |
|||
Flexural Modulus | 8.14 GPa | 1180 ksi | ASTM Data |
BASF Capron® SEG6 H1 BK-122 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron SEG6 H1 BK-122 is a black pigmented, 30% glass reinforced nylon 6 injection molding compound. This material is currently under development as XA-2678. It exhibits exceptional surface aesthet.. |
|||
Flexural Modulus | 8.14 GPa | 1180 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 30G6F Polybutylene terephthalate, 30% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 8.14 GPa | 1180 ksi | ASTM Test |
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Dry) Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, heat stabilized, impact modified, pigmented black, PA6 injection molding compound developed for applications requiring improved dry as molded t.. |
|||
Flexural Modulus | 8.14 GPa | 1180 ksi | ASTM D790 |
Polymer Resources PPX/NY G30 Modified PPO, 30% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 8.14 GPa | 1180 ksi | ASTM D790 |
PlastxWorld CEVIAN® S5230 30% GF PC/ABS alloy Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld .. |