Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM D790 |
Nylene® Naxel™ PC45G FR 10% Glass Reinforced, Flame Retardant Polycarbonate Description: Naxel™ PC45G FR is a 10% glass fiber reinforced, flame retardant polycarbonate. PC45G FR is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins ar.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM D790 |
Polymer Resources PCSF-FR Polycarbonate, 5% Glass Reinforced Structural Foam Grade Polycarbonate, 5% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing cond.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips EA3350 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Medical containersBlends with clear SB-copolymersClam-shell containersBi-axially oriented sheetFeatures:High molecular weight homopolymerHigh Vicat softeni.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM Value |
BASF Capron® 1202CQ Nylon 6 (Dry)
(discontinued **) Capron 1202CQ is a blended low viscosity, polyamide 6 injection molding homopolymer, possessing a modified crystalline structure for increased property performance and faster cycles. It is also ava.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM Data |
BASF Capron® 8200CQ Blend Nylon 6 (Dry)
(discontinued **) Capron 8200CQ Blend is a medium viscosity, nylon 6 injection molding homopolymer possessing the combination of strength, stiffness and toughness properties as well as chemical and abrasion resistanc.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | Tangent; ASTM D790 |
Fiberfil® J-60/15/E Polypropylene Homopolymer, 15% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 8015 PEI High flow Polyetherimide blend. Meets FAR 25.853 and OSU 100/100 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE (Asia Pacific) High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Europe-Africa-Middle East) High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0009E PC (Asia Pacific) LNP* Stat-kon* DD0009E is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790 |
Styron CALIBREâ„¢ 5101-8 Polycarbonate Resin Overview: CALIBREâ„¢ 5101 Polycarbonate resins 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding UL.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM AUT230 PEI Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM D790 |
Chase Plastics CP Pryme® N100HL (Dry) Nylon 6, Heat Stabilized, Lubricated Features: Heat stabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM D790 |
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM D790 |
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM D790 |
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM D790B |
Chevron Phillips EA3400 Medium Flow Crystal DescriptionChevron EA3400 is a medium flow-crystal polystyrene resin developed to blend with Styrene-Butadiene block copolymers for sheet extrusion and vacuum thermoforming. EA3400 can be used in c.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM Test |
BASF Ultramid® 8202C HS PA6 (Dry) Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM Test |
BASF Ultramid® 8202CQ PA6 (Dry) Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme.. |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | |
Asahi Kasei Thermylene® P-30TC-1156 Chemically Coupled Polypropylene Compound, 30% Talc Filled Applications: Automotive: Blower Wheels, HVAC Electrical and Specialty: Flush Valves, Pump BasesInformation provided by Asahi Kasei |
|||
Flexural Modulus | 3.17 GPa | 460 ksi | ASTM D790 |
PolyOne Edgetek® AT-30GB/000 Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledInformation provided by PolyOne Corporation. |