Nylene® Norpex® AX20MR , 20% Mineral Reinforced Polyphenylene Ether

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Mineral Filled
Manufacturer Nylene®
Trade Name Norpex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® Norpex® AX20MR , 20% Mineral Reinforced Polyphenylene Ether.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Norpex® AX20MR is a 20% mineral reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 73.8 MPa
10700 psi
ASTM D638
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648