A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.223 g/cc
1.223 g/cc
ASTM D792
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Flexural Modulus 3.31 GPa
480 ksi
ASTM D790
Izod Impact, Notched 0.260 J/cm
0.487 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 134 °C
273 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C
169 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved