Material Notes:
Provides the highest level of stiffness and heat resistance of filled olefins. Talc filled grades offer the highest strength properties. Typical applications include extrusion/thermoformed food containers, and profile extruded and blown molded structural parts.Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc

@Temperature 22.8 °C
1.05 g/cc

@Temperature 73.0 °F
ASTM D792
Filler Content 20 %
20 %
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
0.125inch wall
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.2 MPa
5100 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Modulus 1.93 GPa
280 ksi
secant; ASTM D790
2.62 GPa
380 ksi
tangent; ASTM D790
Izod Impact, Notched 0.481 J/cm

@Temperature 22.8 °C
0.900 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Gardner Impact >= 1.36 J

@Temperature -5.56 °C
>= 1.00 ft-lb

@Temperature 22.0 °F
ASTM D5420
2.03 J

@Temperature 22.8 °C
1.50 ft-lb

@Temperature 73.0 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.6 °C
150 °F
ASTM D648
Optical Properties Metric English Comments
Gloss 47 %
47 %
60°; ASTM D523