Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hybrid S570 ABS + Polycarbonate Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hybrid
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hybrid S570 ABS + Polycarbonate Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ravago.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Melt Flow 8.5 g/10 min

@Load 2.16 kg,
Temperature 260 °C
8.5 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 61.4 MPa
8900 psi
ASTM D638
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 7.21 J/cm
13.5 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
Unannealed (0.125 in); ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 97.8 °C
208 °F
Unannealed (0.125 in); ASTM D648
Vicat Softening Point 114 °C
237 °F
ASTM D1525
Flammability, UL94 V-0
V-0
0.0600 in, V-0
5VB
5VB
0.0980 in.
5VA
5VA
0.126 in.
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved