Mechanical Properties Metric English Comments
Flexural Modulus 2.38 GPa
345 ksi
Tangent; ASTM D790
RheTech Products GC15P200-00 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Electrical housingsUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.38 GPa
345 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Geloy XTWM206 ASA
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.38 GPa
345 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Geloy XTWM206 ASA (Asia Pacific)
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Asia Pacific regio..
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Polymer Resources ABS-FR Flame Retardant ABS
Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch..
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized
Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and..
Flexural Modulus 2.38 GPa
345 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® 945ASR PC
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Polymer Resources PPX-GP7 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Flexural Modulus 2.38 GPa
345 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® FXM123R PC (Asia Pacific)
FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package ..
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
PolyOne Edgetek® SY-03CF/000 Polystyrene - High Impact (HIPS), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP ABL12 ABS
LNP* Lubricomp* ABL12 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Glass Bead and 5% PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 2.38 GPa
345 ksi
2mm/min; ASTM D790
Kingfa JH830 Flame Retardant PC
Features:UL V-0 @ 1.6mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInformation Prov..
Flexural Modulus 2.38 GPa
345 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Lubricomp ZI001 PPO
LNP* Lubricomp ZI001 is a compound based on Modified PPO containing Silicone. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.38 GPa
345 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON DD200C PC (Asia Pacific)
PTFE free polycarbonate compounds with ESD safety and good lubricating perfomrance , suitable for Semiconductor and Hard Disk Drive (HDD) and semicon industry. Added features of this material includ..
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Star Plastics PC1212FRRUV Molding Grade PC FR
Information provided by Star Plastics, Inc.
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Star Plastics PC1212FRUV Molding Grade PC FR
Information provided by Star Plastics, Inc.
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Star Plastics PC1510FR Molding Grade PC
Information provided by Star Plastics, Inc.
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Star Plastics PC1510UV Molding Grade PC
Information provided by Star Plastics, Inc.
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Star Plastics PC701 Molding Grade PC with release
Information provided by Star Plastics, Inc.
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Star Plastics PC721HFR Molding Grade PC
Information provided by Star Plastics, Inc.
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Star Plastics PC721HFR Molding Grade PC High Flow with Release
Information provided by Star Plastics, Inc.
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Star Plastics PC7523R Molding Grade PC
Information provided by Star Plastics, Inc.
Flexural Modulus 2.38 GPa
345 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DX11354X PC (Asia Pacific)
LNP* Thermocomp* Compound DX11354X is a colorable PC based compound with stable plating and RF performance, colored LDS material solution, good surface and processing window, high impact strength. I..
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Star Plastics PC1212R Molding Grade PC with Release
Information provided by Star Plastics, Inc.
Flexural Modulus 2.38 GPa
345 ksi
ISO 178
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Asia Pacific)
EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor..
Flexural Modulus 2.38 GPa
345 ksi
ISO 178
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Europe-Africa-Middle East)
EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor..
Flexural Modulus 2.38 GPa
345 ksi
ISO 178
Cyclics CBT® 100 Thermoplastic Resin
CBT® 100 resin melts to a water-like viscosity when heated, then polymerizes into the engineering thermoplastic resin polybutylene terephthalate (PBT). CBT 200 resin has a processing range between..
Flexural Modulus 2.38 GPa
345 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ASA S130
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Impact and ModulusInformation provided by Diamond Polymers, Inc.
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Engineered Polymer Solutions ABS 550
Medium Impact. Natural and colors available. Medium gloss. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions.
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Arkema Group Plexiglas® MI7 Acrylic
Plexiglas® MI7 is an impact modified thermoplastic acrylic resin formulated for injection molding and extrusion applications. It is heat resistant, has high melt flow and provides 7 times the impa..
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Polymer Resources PPX-GP5 Modified PPO, General Purpose with HDT of 270 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Copyright © lookpolymers.com All Rights Reserved