Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.38 GPa | 345 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers PC-1029 Description: Natural PolycarbonateInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTWM206 ASA Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | ASTM D790 |
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and.. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® 945ASR PC Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | ASTM D790 |
Polymer Resources PPX-GP5 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 270F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXM123R PC (Asia Pacific) FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package .. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXM123R PC (Europe-Africa-Middle East) FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package .. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Europe-Africa-Middle East) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | Method I (3 point load), Procedure B); ASTM D790 |
Multibase Multi-Pro® 5002 CU Natural Polypropylene Forms:PelletsProcessing Methods:Injection MoldingFeatures:Gloss, LowInformation provided by Multibase |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | ASTM D790 |
PolyOne Edgetek® SY-03CF/000 Polystyrene - High Impact (HIPS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXM123R PC FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package .. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 2mm/min; ASTM D790 |
Kingfa JH830 Flame Retardant PC Features:UL V-0 @ 1.6mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInformation Prov.. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DX07404H PC LNP* LUBRICOMP* DX07404H is a compound based on Polycarbonate containing Proprietary Fillers. Added features of this grade are: Healthcare, Wear Resistant. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DX07404H PC LNP* LUBRICOMP* DX07404H is a compound based on Polycarbonate containing Proprietary Fillers. Added features of this grade are: Healthcare, Wear Resistant. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP ZI001 PPE+PS LNP* LUBRICOMP ZI001 is a compound based on PPE+PS resin containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp ZI001 PPO LNP* Lubricomp ZI001 is a compound based on Modified PPO containing Silicone. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | ASTM D790 |
Star Plastics PC1212FRRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | ASTM D790 |
Star Plastics PC1510FR Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | ASTM D790 |
Star Plastics PC1510R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | ASTM D790 |
Star Plastics PC1510R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | ASTM D790 |
Star Plastics PC1510RUV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX11354X PC (Asia Pacific) LNP* Thermocomp* Compound DX11354X is a colorable PC based compound with stable plating and RF performance, colored LDS material solution, good surface and processing window, high impact strength. I.. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL EN7010 PPE+SEBS (Asia Pacific) High heat, Non halogenated flame retardant Noryl product for Film |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | ISO 178 |
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Asia Pacific) EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor.. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | ISO 178 |
Cyclics CBT® 100 Thermoplastic Resin CBT® 100 resin melts to a water-like viscosity when heated, then polymerizes into the engineering thermoplastic resin polybutylene terephthalate (PBT). CBT 200 resin has a processing range between.. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | ASTM D790 |
Polymer Resources PPX-GP5 Modified PPO, General Purpose with HDT of 270 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 2.38 GPa | 345 ksi | ASTM D790 |
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |