Polymer Property : Flexural Modulus = 8.20 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.80 - 8.20 GPa
261 - 1190 ksi
Average value: 3.18 GPa Grade Count:16
Overview of materials for Acetal Copolymer, Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of..
Flexural Modulus 3.59 - 8.20 GPa
521 - 1190 ksi
Average value: 5.46 GPa Grade Count:7
Overview of materials for Polyphenylene Ether, Glass/Graphite Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Glass/Graphite Reinforced". Each property range of values reported is minimum and m..