Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polyphenylene Ether, Glass/Graphite Reinforced

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Glass/Graphite Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyphenylene Ether, Glass/Graphite Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Glass/Graphite Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.13 - 1.55 g/cc
0.0408 - 0.0560 lb/in³
Average value: 1.31 g/cc Grade Count:7
Filler Content 10.0 - 30.0 %
10.0 - 30.0 %
Average value: 20.0 % Grade Count:6
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 - 110 MPa
10900 - 16000 psi
Average value: 93.5 MPa Grade Count:6
Flexural Modulus 3.59 - 8.20 GPa
521 - 1190 ksi
Average value: 5.46 GPa Grade Count:7
Izod Impact, Notched 0.370 - 1.18 J/cm
0.693 - 2.21 ft-lb/in
Average value: 0.950 J/cm Grade Count:7
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 128 - 141 °C
262 - 286 °F
Average value: 136 °C Grade Count:7
Flammability, UL94 HB - V-1
HB - V-1
Grade Count:6
Electrical Properties Metric English Comments
Dielectric Constant 2.90 - 3.40
2.90 - 3.40
Average value: 3.15 Grade Count:6
Users viewing this material also viewed the following: