Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 520 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
NYCOA 2037 15% Glass Filled Nylon 6
15% glass filled very high viscosity nylon 6Information provided by NYCOA, Inc.
Flexural Modulus 3.59 GPa
520 ksi
Tangent; ASTM D790
RheTech Products F36-01 35% Mica Reinforced Polypropylene Copolymer, Black
Applications: Cowl screensHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 3.59 GPa
520 ksi
Tangent; ASTM D790
RheTech Products G20P100-01 20% Glass Fiber Reinforced Polypropylene, Black
Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Oxford Polymers 25GB-5GF-IM Polybutylene Terephthalate (PBT), Impact Modified/ Glass Beads
Polybutylene Terephthalate (PBT), Impact Modified/ Glass BeadsInformation provided by Oxford Polymers.
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Oxford Polymers PEEK 450-INJ-Black PEEK
Product Description: Polyetheretherketone, general purpose injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon black Special Characteristics: Precol..
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
RTP Company EMI 2262  Polyetheretherketone (PEEK) Shielding - Stainless Steel Fiber 15%  (di
Shielding - Stainless Steel Fiber 15%Comments:EMI/RFI ShieldingESD ProtectionNickel-Coated Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments..
Flexural Modulus 3.59 GPa
520 ksi
ASTM D 790
RTP Company RTP 800 AR 15 Acetal (POM), Aramid Fiber Reinforced
Flexural Modulus 3.59 GPa
520 ksi
ASTM D 790
RTP Company RTP 800 AR 15 TFE 15 Acetal (POM), Aramid Fiber Reinforced - PTFE Lubricated
Flexural Modulus 3.59 GPa
520 ksi
ASTM D 790
RTP Company RTP 800 AR 15 TFE 20 Acetal (POM), Aramid Fiber Reinforced - PTFE Lubricated
Flexural Modulus 3.59 - 29.0 GPa
520 - 4210 ksi
Average value: 11.7 GPa Grade Count:50
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Global GAB-105 5% Glass Reinforced ABS
Information provided by Global Polymers Corporation.
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Global MPP-120-C 20% Mica Reinforced Polypropylene
Information provided by Global Polymers Corporation.
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Techmer ES Electrablend® PC 04006 FR BK Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite..
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Techmer ES Electrablend® PEI 04001 MB Stainless Steel Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc.
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Techmer ES HiFill® PA6 GF10 TL10 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedInf..
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Techmer ES HiFill® PA6 GF10 TL10 BK 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedApp..
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Teknor Apex Sinpolene GPP1620 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 20% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; ..
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Chase Plastics CP Pryme® N120GL (COND, 50% RH) Nylon 6, 20% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Flexural Modulus 3.59 GPa
520 ksi
ASTM D 790
RTP Company EMI 330 G FR Polycarbonate (PC), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Ecomass® 1005ZD96 Tungsten Powder Filled Co-Polyamide, Injection Molding Grade
High Specific Gravity, Tungsten Powder Filled Co-Polyamide (COPA), Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing ..
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Ensinger XP-150 Compression Molded Polyimide Unfilled, Premium Grade
The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal st..
Flexural Modulus 3.59 GPa

@Temperature 22.8 °C
520 ksi

@Temperature 73.0 °F
ASTM D790
Celanese Celanex® 602AC PBT, Glass Reinforced
Celanex 602AC is a 10% fiberglass reinforced PBT that has lower warpage and improved impact over standard PBT.To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a ..
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Asahi Kasei Thermylene® P6-20FG-0659 20% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Asahi Kasei Thermylene® P6-20FG-2153 20% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Asahi Kasei Thermylene® P6-20FG-2153R 20% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Asahi Kasei Thermylene® P6-30FM-Y249B 30% Glass/Mineral Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Asahi Kasei Thermofil P-40TC-0158 40% Talc Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
RTP Company RTP 1801A Z  Polycarbonate/Acrylic Alloy (PC/PMMA) Glass Fiber 10% - FDA Type  (
Glass Fiber 10% - FDA TypeComments:Glass FiberFDA CompliantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided ..
Flexural Modulus 3.59 GPa
520 ksi
Tangent; ASTM D790
RheTech Products GC20P100-00UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Natural
Injection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 3.59 GPa
520 ksi
Tangent; ASTM D790
RheTech Products GC20P105-08FA 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black
Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products.
Copyright © lookpolymers.com All Rights Reserved