Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
Oxford Polymers 30CF 30% Carbon Fiber Reinforced Polyphenylene Sulfide 30% Carbon Fiber Reinforced Polyphenylene SulfideInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
PolyOne Edgetek® PK-30CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | (50.8 mm Span) 1mm/min; ASTM D790 |
LNP VALOX® SMV5847 PBT + PET Alloy, 30% Carbon Fiber Reinforcement
(discontinued **) ESD Applications. VC3000.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data .. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
Mitsui AURUM® JCL3030 Polyimide, Carbon Fiber Filled
(discontinued **) AURUM JCL3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | ASTM D790 |
Quantum Composites QC-7810 55% Glass Fiber Polyester SMC
(discontinued **) QC-7810 is a toughened thermoset polyester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and flame resistance. It is suggested.. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
Techmer ES Electrafil® J-3/CF/30 Nylon 6, 30% Carbon Fiber Reinforced |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
Techmer ES Luriblend® PEI CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF00C is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | ASTM D790 |
Sumitomo Bakelite North America EM 7302LD-2 Long Glass Fiber Reinforced Epoxy EM 7302LD-2 is a long fiberglass reinforced epoxy molding compound with a low density inert filler. This compound is designed for applications where moderate strength and weight savings are desirabl.. |
|||
Flexural Modulus | 17.2 GPa @Temperature 23.0 °C |
2490 ksi @Temperature 73.4 °F |
ASTM D790 |
DuPont Performance Polymers VESPEL TP-8474 Polyimide DuPont Vespel TP-8474 parts are specified for mechanical, thermal, and tribological properties. TP-8474 parts offer excellent strength and toughness, dimensional stability, low outgassing, radiation.. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | ASTM D790 |
PolyOne Edgetek® NI-40CF/000 Nylon 6/10 - 40% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
PolyOne Edgetek® PI-30CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | ASTM D790 |
LATI LARAMID G/50 50% Glass Filled Polyphthalamide (PPA) Based Compound
(Unverified Data**) Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s.. |