Oxford Polymers 30CF 30% Carbon Fiber Reinforced Polyphenylene Sulfide

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler
Manufacturer Oxford Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers 30CF 30% Carbon Fiber Reinforced Polyphenylene Sulfide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Carbon Fiber Reinforced Polyphenylene SulfideInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D792
Filler Content 30 %
30 %
Water Absorption 0.040 %
0.040 %
ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 228 MPa
33000 psi
ASTM D790
Flexural Modulus 17.2 GPa
2500 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Temperature 23.0 °C
1.10 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648