Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 60% Glass Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 60% Glass Reinforced". Specific grades with glass content between 55% and 64% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.77 - 1.80 g/cc
0.0639 - 0.0650 lb/in³
Average value: 1.79 g/cc Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.00200 cm/cm
0.00100 - 0.00200 in/in
Average value: 0.00175 cm/cm Grade Count:3
Mechanical Properties Metric English Comments
Elongation at Break 1.50 - 2.00 %
1.50 - 2.00 %
Average value: 1.67 % Grade Count:3
Flexural Yield Strength 276 - 303 MPa
40000 - 44000 psi
Average value: 290 MPa Grade Count:3
Flexural Modulus 17.2 - 19.3 GPa
2500 - 2800 ksi
Average value: 18.1 GPa Grade Count:3
Izod Impact, Notched 1.01 - 1.12 J/cm
1.90 - 2.10 ft-lb/in
Average value: 1.07 J/cm Grade Count:3
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 229 - 232 °C
444 - 450 °F
Average value: 230 °C Grade Count:3