Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CMT Materials REN Shape® 460 Prototype Tool & Precision Modeling Board

Category Polymer
Manufacturer CMT Materials
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMT Materials REN Shape® 460 Prototype Tool & Precision Modeling Board.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
REN Shape 460 is a moderate density precision modeling board that features a lower coefficient of thermal expansion to provide enhanced dimensional stability over a broader temperature range than other modeling boards. REN Shape 460 provides the same excellent definition and accuracy for which the REN Shape family of products is well known. Machinable with carbide cutters, REN Shape 460 features properties including:Ultra-fine Surface FinishOutstanding Resistance to Shrinkage and WarpingSuperior Reproduction of Intricate DetailApplications: REN 460 applications may include temporary or throw away master models, styling and visual models, prototypes and prototype foundry patters, vacuum form molds, architectural and automotive die models, tooling aids and fixtures, and other applications requiring fast machining and good model surfaces.Information Provided by CMT Materials, Inc.
Physical Properties Metric English Comments
Density 0.769 g/cc
0.0278 lb/in³
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D-2240
Tensile Strength, Ultimate 12.4 MPa
1800 psi
ASTM D-638
Flexural Strength 25.5 MPa
3700 psi
ASTM D-790
Flexural Modulus 1.28 GPa
185 ksi
ASTM D-790
Compressive Strength 15.2 MPa
2200 psi
ASTM D-695
Compressive Modulus 1.25 GPa
181 ksi
ASTM D-695
Thermal Properties Metric English Comments
CTE, linear 53.8 µm/m-°C

@Temperature -30.0 - 30.0 °C
29.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D-3386
Glass Transition Temp, Tg 104 °C
219 °F
ASTM D-4065
Descriptive Properties Value Comments
Color Light Brown
Users viewing this material also viewed the following: