Total PPC 5945WZ Polypropylene, Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Total Atofina
Trade Name PPC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPC 5945WZ Polypropylene, Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TOTAL Petrochemicals Polypropylene 5945WZ is a nucleated impact copolymer with a Melt Flow index of 80 g/10 min.TOTAL Polypropylene 5945WZ is characterized by very low warpage, improved stiffness, and high impact resistance balance, excellent antistatic properties and has been formulated to allow faster cycling through early demolding.Total Polypropylene 5945WZ complies with all applicable FDA regulations for food contact applications.Total Polypropylene 5945WZ has been developed specifically for the injection molding of thin-walled articles and compounding.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D1505
Melt Flow 80 g/10 min
80 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 1.25 GPa
181 ksi
ASTM D790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
TOTAL Method
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
Pressure unspecified, Unannealed; ASTM D648