Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 19.0 J @Temperature -30.0 °C |
14.0 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C4220 PC+ABS PC+ABS Blend with 20% Glass Reinforce. High heat resistance; Excellent balance strength/rigidity; Good impact/appearance. |
|||
Dart Drop, Total Energy | 19.0 J @Temperature 0.000 °C |
14.0 ft-lb @Temperature 32.0 °F |
Instrumented Impact Energy @ peak, @ 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7705 PP SABIC® PPcompound 7705 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, scratch resistance, and heat stability with interior automotive UV stabili.. |
|||
Dart Drop, Total Energy | 19.0 J @Temperature -30.0 °C |
14.0 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak, -30°C @ 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 9710 PP SABIC® PPcompound 9710 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st.. |
|||
Dart Drop, Total Energy | 19.0 J @Temperature 23.0 °C |
14.0 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 9710 PP SABIC® PPcompound 9710 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st.. |
|||
Dart Drop, Total Energy | 19.0 J @Temperature 23.0 °C |
14.0 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 9712 PP SABIC® PPcompound 9712 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st.. |
|||
Dart Drop, Total Energy | 19.0 J @Temperature 23.0 °C |
14.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP 30% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
Dart Drop, Total Energy | 19.0 J @Temperature 23.0 °C |
14.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Asia Pacific) 30% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
Dart Drop, Total Energy | 19.0 J @Temperature -20.0 °C |
14.0 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
ExxonMobil LDPE LD 617.LN Low Density Polyethylene Resin Product Description: LD 617.LN is a high flow, low density polyethylene homopolymer resin designed to provide excellent processability, flexibility and surface appearance. This multipurpose resin is.. |
|||
Dart Drop, Total Energy | 19.0 J @Temperature 22.8 °C |
14.0 ft-lb @Temperature 73.0 °F |
ASTM D3763 |
ExxonMobil LDPE LD 637.LI Low Density Polyethylene Resin Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos.. |
|||
Dart Drop, Total Energy | 19.0 J @Temperature 22.8 °C |
14.0 ft-lb @Temperature 73.0 °F |
ASTM D3763 |
ExxonMobil Escorene™ LD 705.MJ Blown Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 705.MJ is a fractional melt index, 12.8 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and.. |