Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® 5% LF-0718-A in PF-0118-B LDPE Film Resin Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical .. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene CopolymerCharacteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applicationsApplications:Bakery Films, Coextr.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 7120T LLDPE Cast/Blown Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Stretch Wrap, CoextrusionsProcessing Conditio.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882 |
NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Strength and toughness, good sealing properties, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 5554-D LDPE High Clarity, Medium Impact, Low Slip Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Clarity, Good Impact Strength, Good Sealability, Low SlipApplications:Food Packaging, Case Shrink Wrap, LaminationsProcessing Conditions: Extruder 6.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 5758 LDPE High Clarity, High Impact Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: High Clarity, Excellent Impact Strength, Medium Slip, Medium Antiblock, Moderately High Coefficient of Friction, Easy Openability of BagsApplications:Case Shr.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | 0.01; ASTM D882 |
Eastman 1925F Polyethylene Film
(discontinued **) Polyethylene 1925F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | 1% Secant; ASTM D882 |
Eastman E6838-795F Polyethylene
(discontinued **) E6838-795F is a low density formulation with no slip or antiblock level. It is suggested for film applications that require a good balance of properties such as converter film for industrial packag.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | 1% Secant; ASTM D882 |
Eastman E6838-796F Polyethylene
(discontinued **) E6838-796F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial packaging, gen.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882 |
ExxonMobil Escorene® LD-103 LDPE Industrial Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer industrial film resin with excellent toughness. LD-103 has a low melt index which gives excellent impact strength and melt strength o.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Huntsman PE5030 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Good draw down, low neck-in, good heat sealability and adhesion, low smoking, and excellent printabilityApplications: Extrusion: coating grade and general coa.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Huntsman PE5032 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, excellent heat sealability, good adhesion, low smoking, no edge weave, and excellent printability.Applications: Extrusion: c.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882 |
ExxonMobil Escorene® LD-334 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 4.2% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882-A |
Borealis Himod™ FT6273 LDPE for Film Himod FT6273 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882-A |
Borealis Himod™ FT6274 LDPE for Film Himod FT6274 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 5754 LDPE High Clarity, High Impact Film Resin for General Purpose Packaging Resin Type: HomopolymerCharacteristics: Excellent Impact Strength, High Clarity, Medium Slip, Medium Antiblock, Low Coefficient of Friction, Good OpenabilityApplications:Heavy Produce Bags, Frozen F.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips MarFlex® 5755 LDPE High Clarity, High Impact Film Resin Resin Type: HomopolymerCharacteristics: High Clarity, Excellent Impact Strength, Medium Slip, High Antiblock, Moderately High Coefficient of Friction, Excellent ProcessabilityApplications:Case Shrin.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 6335B LLDPE Cast/Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, Medium Slip Version of 6335Characteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applications, Lo.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | ASTM D882 |
NOVA Chemicals Sclair® 11M1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, strength and toughness.Applications: Co-extrusion.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | 1% Secant; ASTM D882 |
Eastman D4036-F Polyethylene
(discontinued **) D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener.. |
|||
Secant Modulus, TD | 0.220 GPa | 31.9 ksi | 1% Secant; ASTM D882 |
Eastman E6838-963F Polyethylene
(discontinued **) E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati.. |