Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips 5754 LDPE High Clarity, High Impact Film Resin for General Purpose Packaging

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips 5754 LDPE High Clarity, High Impact Film Resin for General Purpose Packaging.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: HomopolymerCharacteristics: Excellent Impact Strength, High Clarity, Medium Slip, Medium Antiblock, Low Coefficient of Friction, Good OpenabilityApplications:Heavy Produce Bags, Frozen Foods Packaging, Dry Goods PackagingProcessing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Blow-Up Ratio 2:1.Film properties below based on film thickness of 31.8 µm.Data provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ASTM D1505
Melt Flow 0.80 g/10 min
0.80 g/10 min
Condition E; ASTM D 1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.190 GPa
27.6 ksi
ASTM D882
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
Coefficient of Friction 0.10
0.10
ASTM D1894
Dart Drop 3.10 g/micron
78.7 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Optical Properties Metric English Comments
Haze 5.0 %
5.0 %
ASTM D2457
Gloss 70 %
70 %
at 45°. ASTM D 2457
110 %
110 %
at 60°. ASTM D 2457
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 204 °C
399 °F