Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Himod™ FT6274 LDPE for Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Borealis
Trade Name Himod™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Himod™ FT6274 LDPE for Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Himod FT6274 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and improved optical properties. Benefits can be obtained in terms of better down gauging possibilities and improved processability. Excellent printing quality is obtained due to high clarity and better layout.Himod FT6274 is intended for applications like: fine shrink films with higher stiffness and transparency, stiff films with excellent optical properties for automated packaging machinery, and lamination film/food packaging.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.927 g/cc
0.0335 lb/in³
ISO 1183
Thickness 40.0 microns
1.57 mil
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Antiblock Level 750 ppm
750 ppm
Additive - Synthetic Silica
Slip Level 300 ppm
300 ppm
Additive - Erucamide
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 230 %
230 %
ISO 527-3
Film Elongation at Break, TD 550 %
550 %
ISO 527-3
Secant Modulus, MD 0.190 GPa
27.6 ksi
ASTM D882-A
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882-A
Impact 33.5
33.5
Puncture Resistance, force (N); ASTM D5748
Puncture Energy 0.500 J
0.369 ft-lb
ASTM D5748
Coefficient of Friction, Dynamic 0.20
0.20
ISO 8295
Tear Strength, Total 2.50 N
0.562 lb (f)
TD; ISO 6383/2
4.00 N
0.899 lb (f)
MD; ISO 6383/2
Dart Drop 2.25 g/micron
57.1 g/mil
ISO 7765/1
Film Tensile Strength at Break, MD 24.0 MPa
3480 psi
ISO 527-3
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 116 °C
241 °F
ISO 11357/03
Vicat Softening Point 101 °C
214 °F
A (10N); ISO 306
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Gloss 105 %
105 %
ASTM D2457
Users viewing this material also viewed the following: