Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips 5758 LDPE High Clarity, High Impact Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips 5758 LDPE High Clarity, High Impact Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: HomopolymerCharacteristics: High Clarity, Excellent Impact Strength, Medium Slip, Medium Antiblock, Moderately High Coefficient of Friction, Easy Openability of BagsApplications:Case Shrink Wrap, Bundling, Laminations, Diaper Liners, Frozen Food, Heavy Produce, Hardware PackagingProcessing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Blow-Up Ratio 2:1.Film properties below based on film thickness of 31.8 µm.Data provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D1505
Melt Flow 0.80 g/10 min
0.80 g/10 min
Condition E; ASTM D 1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.190 GPa
27.6 ksi
ASTM D882
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
Coefficient of Friction >= 0.60
>= 0.60
ASTM D1894
Dart Drop 3.10 g/micron
78.7 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D2457
Gloss 65 %
65 %
at 45°. ASTM D 2457
100 %
100 %
at 60°. ASTM D 2457
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 204 °C
399 °F
Copyright © lookpolymers.com All Rights Reserved