Polymer Property : Shear Strength = 7.93 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 7.93 MPa

@Thickness 1.57 mm
1150 psi

@Thickness 0.0620 in
Perpendicular
Industrial Laminates/Norplex NP631 Paper Base Laminate
Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500"
Shear Strength 7.93 MPa
1150 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 1/16-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 7.93 MPa
1150 psi
Overlap, PP, Substrate Failure
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 7.93 MPa

@Temperature 66.0 °C
1150 psi

@Temperature 151 °F
Overlap, HDPE, AF/CF
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 7.93 MPa
1150 psi
Overlap, PP, Substrate Failure
3M Scotch-Weld™ DP8010NS Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop..
Shear Strength 7.93 MPa
1150 psi
Overlap, Plexiglass (PMMA), Substrate Failure
3M Scotch-Weld™ DP8010NS Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop..
Shear Strength 7.93 MPa
1150 psi
Overlap at 20 minutes after bonding
3M Scotch-Weld™ DP810 Black Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 7.93 MPa

@Temperature 66.0 °C
1150 psi

@Temperature 151 °F
Overlap, Oak, Substrate/Adhesive Failure
3M Scotch-Weld™ Thin Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 7.93 MPa
1150 psi
Overlap, Polycarbonate
3M Scotch-Weld™ DP820 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Shear Strength 7.93 MPa
1150 psi
Overlap, CRS (oily) 49°C/100% RH/2 wks
3M Scotch-Weld™ DP820 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..