Mechanical Properties Metric English Comments
Shear Strength >= 0.345 MPa
>= 50.0 psi
Parker Chomerics Tecknit® 0035 Conductive Silicone Sealant/Adhesive
Comments: Thin flexible pasteTypical Applications: Bonding elastomer gasketInformation provided by Chomerics
Shear Strength >= 0.345 MPa
>= 50.0 psi
Cured; ASTM D1002
Parker Chomerics Tecknit CON/RTV-Ni 2 Part Nickel Filled RTV
Description: TECKNIT electrically conductive, medium viscosity adhesive- sealant system. It is formulated with a special conductive material producing its own unique advantages. After full cure, the..
Shear Strength >= 0.345 MPa
>= 50.0 psi
Bond, Al to Al
Master Bond MasterSil 151Med Medical Grade Silicone Potting Compound
Description: Master Bond MasterSil 151Med is a two component, low viscosity silicone compound for high performance potting and encapsulation. MasterSil 151Med is an addition cured system and does no..
Shear Strength 0.345 MPa
50.0 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 3/8-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength >= 0.345 MPa
>= 50.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRH-10/OX - 3/16 - 1.8 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength >= 0.345 MPa
>= 50.0 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRH-49 - 1/4 - 2.1 Woven Kevlar Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-49 is manufactured using KEVLAR® 49 fabric. A thermosetting adhesive is used for the node bonds and a 350°F cure modified epoxy resin i..
Shear Strength 0.345 MPa
50.0 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 1/4-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength >= 0.345 MPa
>= 50.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® CR III 3/16-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 0.345 MPa
50.0 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 0.345 MPa
50.0 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10 - 1/4 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength 0.345 MPa
50.0 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10 - 1/8- 1.8 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength 0.345 MPa
50.0 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10 - 3/16 - 1.8 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength >= 0.345 MPa
>= 50.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRH-10/F35 - 2.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Shear Strength >= 0.345 MPa
>= 50.0 psi
Plate Shear, L Direction, minimum individual
Hexcel® HexWeb® HRH-310 - 1/8 - 1.8 Aramid Fiber/Polyimide Resin Honeycomb
Designation: Material-Cell Size-DensityHexWeb HRH-310 is manufactured from aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the hexagon..
Shear Strength 0.345 MPa
50.0 psi
Polycarbonate, 180°, after 48 hrs at 23°C
3M Fastbond™ 4224-NF Pressure Sensitive Adhesives
3M™ Fastbond™ Pressure Sensitive Adhesive 4224-NF is a water-based, permanently pressure sensitive adhesive with excellent initial tack and good bond strength.Information provided by 3M
Shear Strength 0.345 MPa
50.0 psi
ABS Plastic, after 48 hrs at 23°C
3M Fastbond™ 49 Insulation Adhesive
3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and ..
Shear Strength 0.345 MPa
50.0 psi
Overlap, Polypropylene
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro..
Shear Strength 0.345 MPa
50.0 psi
Overlap, Toluene for 14 days, Cohesive Failure
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 0.345 MPa
50.0 psi
Overlap, Toluene for 14 days, Cohesive Failure
3M Scotch-Weld™ DP8010 Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl..
Shear Strength 0.345 MPa
50.0 psi
Overlap, Toluene for 14 days, Cohesive Failure
3M Scotch-Weld™ DP8010NS Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop..
Shear Strength 0.345 MPa
50.0 psi
Overlap, Acetone for 14 days, Cohesive Failure
3M Scotch-Weld™ DP810 Black Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 0.345 MPa
50.0 psi
Overlap, MEK for 14 days, Cohesive Failure
3M Scotch-Weld™ DP810 Tan Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 0.345 MPa
50.0 psi
Overlap at 10 minutes after bonding
3M Scotch-Weld™ DP810 Tan Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..