Polymer Property : Shear Strength = 0.827 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength >= 0.827 MPa
>= 120 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® CR III 5/32-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 0.827 MPa
120 psi
Plate Shear, W Direction
Hexcel® HexWeb® HRH-36 - 1/8 - 3.0 Para-Aramid/Phenolic Core
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low..
Shear Strength 0.827 MPa
120 psi
Plate Shear, L Direction
Hexcel® HexWeb® HRH-36 - 3/16 - 2.0 Para-Aramid/Phenolic Core
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low..
Shear Strength 0.827 MPa
120 psi
Plate Shear, L Direction
Hexcel® HexWeb® HRH-78 - 1/4 - 3.0 Commercial Grade Nomex Honeycomb/Phenolic Resin
Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after..
Shear Strength 0.827 MPa
120 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRP - 3/8 - 2.2 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength 0.827 MPa
120 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRP - 3/8 - 3.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength >= 0.827 MPa
>= 120 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRP/OX - 3/8 - 3.2 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength 0.827 MPa
120 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10/F35 - 3.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Shear Strength 0.827 MPa
120 psi
Overlap, Neoprene Rubber; ASTM D1002-64
3M Scotch-Weld™ CA100 Instant Adhesive
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. High-peel and impact strength and high thermal shock and heat resistance.Information provided by 3M..
Shear Strength 0.827 MPa
120 psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Neoprene/Steel
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 0.827 MPa
120 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 3/16-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..