Hexcel® HexWeb® HRH-36 - 3/16 - 2.0 Para-Aramid/Phenolic Core

Category Other Engineering Material , Composite Core Material , Polymer , Thermoset , Aramid , Phenolic
Manufacturer Hexcel
Trade Name HexWeb®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexWeb® HRH-36 - 3/16 - 2.0 Para-Aramid/Phenolic Core.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low moisture pickup; Excellent thermal stability; Smooth cell wall finish.Applications: HexWeb® HRH-36 is a high performance non-metallic core, available in a wide range of densities, suitable for most composite sandwich applications. It can be readily heat formed to help produce complex components and offers similar mechanical properties to KOREX® core as well as comparable moisture pickup. In addition, HexWeb® HRH-36 offers a weight reduction over higher density NOMEX® honeycomb cores.
Physical Properties Metric English Comments
Density 0.0320 g/cc
0.00116 lb/in³
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.965 MPa
140 psi
Bare
1.10 MPa
160 psi
Stabilized
Shear Modulus 0.0338 GPa
4.90 ksi
Plate Shear, W Direction
0.0689 GPa
10.0 ksi
Plate Shear, L Direction
Shear Strength 0.483 MPa
70.0 psi
Plate Shear, W Direction
0.827 MPa
120 psi
Plate Shear, L Direction