Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop = 11.0 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 2.00 - 11.0 g/micron
50.8 - 279 g/mil
Average value: 3.48 g/micron Grade Count:24
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and..