Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 770 g | 770 g | ASTM D1922 |
ExxonMobil Enable™ 27-03CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Elmendorf Tear Strength TD | 770 g | 770 g | ASTM D1922 |
ExxonMobil Pax-Plus™ 3201 Blown Film Resin Pax-Plus 3201 is a rubber modified high density polyethylene film resin that exhibits excellent impact strength and stress crack resistance. It is used primarily in film where its good tear resista.. |
|||
Elmendorf Tear Strength TD | 770 g | 770 g | Unspecified film thickness |
Dow Elite® 5400 Linear Low Density Polyethylene 5400 enhanced polyethylene resin is a copolymer produced via INSITE technology from Dow Plastics. It offers extremely high impact resistance, combined with excellent tear, tensile, and optical prop.. |
|||
Elmendorf Tear Strength TD | 770 g | 770 g | ASTM-D1922 |
Braskem LL5800N LLDPE Blown Film Extrusion Polyethylene Copolymer LL5800N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing aid .. |
|||
Elmendorf Tear Strength TD | 770 g | 770 g | ASTM-D1922 |
Braskem LL5801N LLDPE Blown Film Extrusion Polyethylene Copolymer The LL5801N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing .. |
|||
Elmendorf Tear Strength TD | 770 g | 770 g | ASTM D1922 |
ExxonMobil Escorene® LL-3003 LLDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3003 have outstanding tensile properties as well as stiffness and toughness.Applicatio.. |