Material Notes:
Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and puncture. Easier processing and excellent properties lead to significant high pressure LDPE replacement in many applications, yet with superior drawdown and enhanced toughness. Availability: Africa & Middle East, Asia Pacific and EuropeAdditive:Antiblock: NoSlip: NoProcessing Aid: YesThermal Stabilizer: YesApplications:Blown FilmCollation ShrinkFood packagingForm Fill and Seal PackagingHeavy Duty BagsLamination FilmMultilayer Packaging FilmShrink FilmStand Up Pouches Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.927 g/cc
0.0335 lb/in³
ExxonMobil method
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 13.1 MPa
1900 psi
ASTM D882
Film Tensile Strength at Yield, TD 15.2 MPa
2200 psi
ASTM D882
Film Elongation at Break, MD 470 %
470 %
ASTM D882
Film Elongation at Break, TD 760 %
760 %
ASTM D882
Puncture Energy 3.50 J
2.58 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 40 g
40 g
ASTM D1922
Elmendorf Tear Strength TD 770 g
770 g
ASTM D1922
Dart Drop Test 130 g
0.287 lb
ASTM D1709
Film Tensile Strength at Break, MD 66.2 MPa
9600 psi
ASTM D882
Film Tensile Strength at Break, TD 53.1 MPa
7700 psi
ASTM D882
1% Secant Modulus, MD 310 MPa
45000 psi
ASTM D882
1% Secant Modulus, TD 365 MPa
53000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 246 °C
<= 475 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 12 %
12 %
ASTM D1003
Gloss 45 %
45 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 11 lbf
ExxonMobil Method