Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 35.0 - 58.0 MPa | 5080 - 8410 psi | Average value: 45.0 MPa Grade Count:28 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Ultimate | 41.0 - 58.0 MPa | 5950 - 8410 psi | Average value: 50.1 MPa Grade Count:10 |
Overview of materials for Phenolic, Novolac, Fabric Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Strength, Ultimate | 50.0 - 58.0 MPa | 7250 - 8410 psi | Average value: 55.3 MPa Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Strength, Ultimate | 51.1 - 58.0 MPa | 7410 - 8410 psi | Average value: 54.0 MPa Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v.. |