Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 462 - 503 MPa | 67000 - 73000 psi | |
Eagle Brass 194 HSM® Copper, Extra Hard High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Strength, Ultimate | 400 - 503 MPa | 58000 - 73000 psi | |
Eagle Brass 510 Phosphor Bronzes 5% A, 1/2 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |