Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 38.2 MPa
5550 psi
DIN 53455; ASTM D638
Kolon KOLEFIN® KO133MT40 M/F Reinforced Polypropylene
KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica..
Tensile Strength, Ultimate 38.2 MPa
5550 psi
ASTM D638
Global F-7000 High Density Polyethylene
Description-high quality is suitable for blown film @wide range of size & thickness Applications-large & small rolled film, shopping bag, merchant bag, disposal waste bagInformation provided by Glob..
Tensile Strength, Ultimate 38.2 MPa
5550 psi
ASTM D638
Global F-8000 High Density Polyethylene
Description-good mechanical strengthApplications-blown wide film applications producing liner film & industrial filmInformation provided by Global Polymers Corporation.
Tensile Strength, Ultimate 38.2 MPa
5550 psi
ASTM D638
Global S-5000 High Density Polyethylene
Description-good for monofilament Applications-ropes, fishing net, agricultural net and sports netInformation provided by Global Polymers Corporation.
Tensile Strength, Ultimate 38.2 MPa
5550 psi
ASTM D638
SK Chemicals SKYPEL G155D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tensile Strength, Ultimate 38.2 MPa
5550 psi
ASTM D638
SK Chemicals SKYPEL M555DH General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tensile Strength, Ultimate 38.2 MPa
5550 psi
ASTM D412
SK Chemicals SKYTHANE® S398A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 38.2 MPa
5540 psi
ASTM D1238
Lubrizol Estane® 2103-90AE Thermoplastic Polyurethane Elastomer
Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Tensile Strength, Ultimate 38.2 MPa
5550 psi
ASTM D412
SK Chemicals SKYTHANE® 398A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..