Kolon KOLEFIN® KO133MT40 M/F Reinforced Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer Kolon
Trade Name KOLEFIN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon KOLEFIN® KO133MT40 M/F Reinforced Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanical properties and for high heat resistance, low mold shrinkage, good processabilityInformation provided by US distributor, API-Kolon.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
DIN 53479; ASTM D792
Water Absorption 0.20 %
0.20 %
DIN 53475; ASTM D570
Linear Mold Shrinkage 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
DIN 53505; ASTM D785
Tensile Strength, Ultimate 38.2 MPa
5550 psi
DIN 53455; ASTM D638
Elongation at Break 30 %
30 %
DIN 53455; ASTM D638
Flexural Yield Strength 59.8 MPa
8680 psi
DIN 53455; ASTM D790
Flexural Modulus 3.63 GPa
526 ksi
DIN 53452; ASTM D790
Izod Impact, Notched 0.343 J/cm
0.643 ft-lb/in
DIN 53453; ASTM D256
Thermal Properties Metric English Comments
Melting Point 170 °C
338 °F
DIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
DIN 53461; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 28.0 kV/mm
711 kV/in
ASTM D149/DIN 53481
Arc Resistance 130 sec
130 sec
ASTM D495