Material Notes:
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plastics to low hardness rubber. It is a kind of thermoplastic elastomer, which can be molded with general plastic mold by plasticizing at high temperature.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Water Absorption 0.70 %
0.70 %
24 hour; ASTM D570
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength, Ultimate 38.2 MPa
5550 psi
ASTM D638
Tensile Strength, Yield 6.37 MPa

@Strain 5.00 %
925 psi

@Strain 5.00 %
ASTM D638
11.3 MPa

@Strain 10.0 %
1640 psi

@Strain 10.0 %
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Flexural Modulus 0.206 GPa
29.9 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Tear Strength 160 kN/m
913 pli
ASTM D1004
Thermal Properties Metric English Comments
Melting Point 202 °C
396 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
ASTM D648