Material Notes:
Description-good mechanical strengthApplications-blown wide film applications producing liner film & industrial filmInformation provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 600 hour
600 hour
ASTM D1693
Melt Flow 0.030 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.030 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D2240
Tensile Strength, Ultimate 38.2 MPa
5550 psi
ASTM D638
Tensile Strength, Yield 22.6 MPa
3270 psi
ASTM D638
Elongation at Break 700 %
700 %
ASTM D638
Flexural Modulus 0.735 GPa
107 ksi
Olsen Stiffness; ASTM D747
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 131 °C
268 °F
ASTM D2117
Vicat Softening Point 125 °C
257 °F
ASTM D1525