SK Chemicals SKYPEL G155D General Grade

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP
Manufacturer SK Chemicals
Trade Name SKYPEL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYPEL G155D General Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plastics to low hardness rubber. It is a kind of thermoplastic elastomer, which can be molded with general plastic mold by plasticizing at high temperature.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Water Absorption 0.50 %
0.50 %
24 hour; ASTM D570
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 220 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength, Ultimate 38.2 MPa
5550 psi
ASTM D638
Tensile Strength, Yield 7.35 MPa

@Strain 5.00 %
1070 psi

@Strain 5.00 %
ASTM D638
12.3 MPa

@Strain 10.0 %
1780 psi

@Strain 10.0 %
ASTM D638
Elongation at Break 550 %
550 %
ASTM D638
Flexural Modulus 0.206 GPa
29.9 ksi
ASTM D790
Resilience 55
55
ASTM D2632
Izod Impact, Notched NB
NB
ASTM D256
Tear Strength 165 kN/m
941 pli
ASTM D1004
Thermal Properties Metric English Comments
Melting Point 202 °C
396 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648