Dymax 9-20557 Conformal Coating

Category Polymer , Adhesive , Thermoset
Manufacturer Dymax Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dymax 9-20557 Conformal Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-20557 Conformal CoatingFlexible and tough with superior adhesion to a wide range of boards and masks; excellent thermal shock resistance. Cure Speed (fpm): 2 - 5 Cure Type: UV/Visible and Heat
Physical Properties Metric English Comments
Viscosity 2500 cP
2500 cP
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.7 MPa
3000 psi
Descriptive Properties Value Comments
Cure Depth 0.25 in.