PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-running situations, leak-tight material, greater durability, less wear debris – runs cleaner, broader resistance to chemical attack, suitable for fluid and gas applications, lapping of seal face not necessary, and exceptionally stable.
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
ASTM-D792
Deformation 11 %

@Pressure 13.8 MPa,
Temperature 25.6 °C
11 %

@Pressure 2000 psi,
Temperature 78.0 °F
24 hrs.; ASTM-D621
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.7 MPa
3000 psi
ASTM-D1457
Elongation at Break 250 %
250 %
ASTM-D1457
Flexural Strength 17.9 MPa
2600 psi
ASTM-F417
Flexural Modulus 0.0621 GPa
9.00 ksi
ASTM-D790
Compressive Strength 42.7 MPa
6200 psi
ASTM-C773
Thermal Properties Metric English Comments
CTE, linear 13.5 µm/m-°C
7.50 µin/in-°F
ASTM-D696
Thermal Conductivity 0.403 W/m-K
2.80 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
500 °F
Descriptive Properties Value Comments
Color Black