Polymer Property : Tensile Strength, Ultimate = 26100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 40.0 - 180 MPa
5800 - 26100 psi
Average value: 146 MPa Grade Count:26
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Tensile Strength, Ultimate 2.70 - 180 MPa
392 - 26100 psi
Average value: 77.9 MPa Grade Count:49
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Tensile Strength, Ultimate 70.0 - 180 MPa

@Temperature 125 - 275 °C
10200 - 26100 psi

@Temperature 257 - 527 °F
Average value: 123 MPa Grade Count:1
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported ..
Tensile Strength, Ultimate 34.5 - 180 MPa
5000 - 26100 psi
Average value: 93.7 MPa Grade Count:36
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% ..
Tensile Strength, Ultimate 115 - 180 MPa

@Temperature 70.0 - 175 °C
16700 - 26100 psi

@Temperature 158 - 347 °F
Average value: 139 MPa Grade Count:4
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Tensile Strength, Ultimate 115 - 180 MPa

@Time 180000 - 7.20e+7 sec
16700 - 26100 psi

@Time 50.0 - 20000 hour
Average value: 139 MPa Grade Count:4
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Tensile Strength, Ultimate 25.9 - 180 MPa
3760 - 26100 psi
Average value: 114 MPa Grade Count:183
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Tensile Strength, Ultimate 13.8 - 180 MPa
2000 - 26100 psi
Average value: 105 MPa Grade Count:277
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..
Tensile Strength, Ultimate 59.2949 - 180 MPa

@Temperature -40.0 - 204 °C
8600.01 - 26100 psi

@Temperature -40.0 - 400 °F
Average value: 115 MPa Grade Count:5
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
Tensile Strength, Ultimate 41.1 - 180 MPa
5960 - 26100 psi
Average value: 111 MPa Grade Count:52
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..