Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® MLS-195A Polysulfone Alloy - ESD Material  (discontinued **)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® MLS-195A Polysulfone Alloy - ESD Material  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0025 cm/cm

@Thickness 3.17 mm
0.0020 - 0.0025 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 107 MPa
15500 psi
ASTM D638
Elongation at Break 3.0 - 4.0 %
3.0 - 4.0 %
ASTM D638
Tensile Modulus 6.20 GPa
899 ksi
ASTM D638
Izod Impact, Notched 0.800 J/cm

@Thickness 6.35 mm
1.50 ft-lb/in

@Thickness 0.250 in
ASTM D256
Electrical Properties Metric English Comments
Electrical Resistivity 10000 ohm-cm - 1e+05
10000 ohm-cm - 1e+05
ASTM D257
Surface Resistance 1e+05 - 5.00e+7 ohm
1e+05 - 5.00e+7 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 332 - 349 °C
630 - 660 °F
Stock
Mold Temperature 66.0 - 121 °C
151 - 250 °F
Drying Temperature 121 - 132 °C
250 - 270 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved