Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chem Polymer Chemlon 214 G Nylon 6, 14% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 10% Glass Fiber Filled
Manufacturer Chem Polymer
Trade Name Chemlon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Chemlon 214 G Nylon 6, 14% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 14% glass fiber reinforced nylon 6 offering improved creep resistance, stiffness, tensile and dimensional stability over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 107 MPa
15500 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Yield Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 4.10 GPa
595 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 246 °C
475 °F
Users viewing this material also viewed the following: