Polymer Property : Tensile Strength, Ultimate = 106.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 106.9 MPa
15500 psi
ASTM D638
PTS Trimid® N66-G13LU 13% Glass Fiber Reinforced Utility Lubricated Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).