Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.924 - 0.945 g/cc
0.0334 - 0.0341 lb/in³
Average value: 0.937 g/cc Grade Count:67
Environmental Stress Crack Resistance 10.0 - 1000 hour
10.0 - 1000 hour
Average value: 376 hour Grade Count:25
>= 1000 hour

@Temperature 50.0 - 50.0 °C
>= 1000 hour

@Temperature 122 - 122 °F
Average value: 1000 hour Grade Count:1
Melt Flow 2.00 - 50.0 g/10 min
2.00 - 50.0 g/10 min
Average value: 6.30 g/10 min Grade Count:67
Mechanical Properties Metric English Comments
Hardness, Shore D 50.0 - 67.0
50.0 - 67.0
Average value: 56.6 Grade Count:55
Tensile Strength, Ultimate 11.7 - 27.1 MPa
1700 - 3930 psi
Average value: 19.5 MPa Grade Count:10
Tensile Strength, Yield 11.0 - 22.0 MPa
1600 - 3190 psi
Average value: 18.1 MPa Grade Count:66
Elongation at Break 150 - 1000 %
150 - 1000 %
Average value: 563 % Grade Count:64
Elongation at Yield 10.0 - 12.0 %
10.0 - 12.0 %
Average value: 11.2 % Grade Count:8
Flexural Modulus 0.317 - 0.931 GPa
46.0 - 135 ksi
Average value: 0.630 GPa Grade Count:67
Falling Dart Impact 27.1164 - 65.0794 J

@Temperature -40.0 - -40.0 °C
20.0000 - 48.0001 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 46.1 J Grade Count:2
Dart Drop Total Energy 200 - 220 J/cm
0.375 - 0.412 ft-lb/mil
Average value: 208 J/cm Grade Count:4
Thermal Properties Metric English Comments
Melting Point 125 - 128 °C
257 - 262 °F
Average value: 126 °C Grade Count:11
Deflection Temperature at 0.46 MPa (66 psi) 49.0 - 60.0 °C
120 - 140 °F
Average value: 54.4 °C Grade Count:13
Deflection Temperature at 1.8 MPa (264 psi) 37.0 - 42.0 °C
98.6 - 108 °F
Average value: 39.1 °C Grade Count:7
Vicat Softening Point 113 - 121 °C
235 - 250 °F
Average value: 117 °C Grade Count:6
Brittleness Temperature -71.0 - -70.0 °C
-95.8 - -94.0 °F
Average value: -70.2 °C Grade Count:5
Optical Properties Metric English Comments
Transmission, Visible 90.0 %
90.0 %
Average value: 90.0 % Grade Count:4