Mechanical Properties Metric English Comments
Dart Drop, Total Energy 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycolac® FR15U ABS
Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60).
Dart Drop, Total Energy 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific)
Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing.
Dart Drop, Total Energy 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycolac® MG29 ABS
Super high impact ABS. Good low temperature toughness. High gloss.
Dart Drop, Total Energy 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycolac® MG29 ABS (Asia Pacific)
Super high impact ABS. Good low temperature toughness. High gloss.
Dart Drop, Total Energy 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® ML7672 PC (Asia Pacific)
Non FR PC + GF, UV-Stabilizer, balanced flow & impact. Available in Opaque only.
Dart Drop, Total Energy 28.0 J
20.7 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated.
Dart Drop, Total Energy 28.0 J
20.7 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific)
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.
Dart Drop, Total Energy 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics ULTEM HU1110 PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
Dart Drop, Total Energy 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics ULTEM HU1110 PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
Dart Drop, Total Energy 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics ULTEM HU2400 PEI
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food..
Dart Drop, Total Energy 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics ULTEM HU2400 PEI (Asia Pacific)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food..
Dart Drop, Total Energy 28.0 J
20.7 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-LOY K3000Z Acetal
LNP* STAT-LOY* K3000Z is a compound based on unfilled Acetal resin. Added feature of this material is: Antistat.
Dart Drop, Total Energy 28.0 J

@Thickness 0.0500 mm
20.7 ft-lb

@Thickness 0.00197 in
1150N; ISO 7765-2
Borealis BD212CF Polypropylene Copolymer
BD212CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BD212CF is designed for food packaging, l..
Dart Drop, Total Energy 28.0 J
20.7 ft-lb
1050N; ISO 7765-2
Borealis Bormed™ TD109CF Polypropylene Copolymer
Bormed™ TD109CF is a propylene alpha olefin copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: lamination films, food..