Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Bormed™ TD109CF Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name Bormed™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Bormed™ TD109CF Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bormed™ TD109CF is a propylene alpha olefin copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: lamination films, food packaging, medical applications, sealing layer in coextrusion. Bormed™ TD109CF does not contain slip or antiblock additives.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.900 - 0.910 g/cc
0.0325 - 0.0329 lb/in³
ISO 1183
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 400 - 500 %
400 - 500 %
MD/TD; ISO 527-3
Tensile Modulus 0.650 - 0.850 GPa
94.3 - 123 ksi
MD/TD; ISO 527-3
Flexural Modulus 0.700 GPa
102 ksi
ISO 178
Dart Drop, Total Energy 28.0 J
20.7 ft-lb
1050N; ISO 7765-2
Coefficient of Friction >= 0.70
>= 0.70
film to film; ISO 8295
Film Tensile Strength at Break, MD 45.0 - 55.0 MPa
6530 - 7980 psi
ISO 527-3
Film Tensile Strength at Break, TD 35.0 - 45.0 MPa
5080 - 6530 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 128 - 132 °C
262 - 270 °F
ISO 3146
Vicat Softening Point 114 °C
237 °F
ISO 306
Optical Properties Metric English Comments
Haze <= 1.3 %
<= 1.3 %
ASTM D1003
Gloss >= 135 %
>= 135 %
20° of arc; ASTM D2457
Copyright © lookpolymers.com All Rights Reserved