Material Notes:
LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 30.0 J
22.1 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 99.0 J
73.0 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 142 °C
288 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
141 °C

@Thickness 3.20 mm
286 °F

@Thickness 0.126 in
unannealed; ASTM D648