Material Notes:
3M™ Scotch-Weld™ Neoprene Contact Adhesive 10 is a multi-purpose contact adhesive which may be used to bond plastic laminate, aluminum, steel, wallboard, wood, masonry, rubber and canvas.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 21 - 25 %
21 - 25 %
Brookfield Viscosity 450 - 700 cP
450 - 700 cP
RVF #2 sp @ 20 rpm @ 80°F
Mechanical Properties Metric English Comments
Shear Strength 0.483 MPa

@Temperature 107 °C,
Time 1.81e+6 sec
70.0 psi

@Temperature 225 °F,
Time 504 hour
Overlap
0.765 MPa

@Temperature 82.0 °C,
Time 1.81e+6 sec
111 psi

@Temperature 180 °F,
Time 504 hour
Overlap
2.96 MPa

@Temperature 75.0 °C,
Time 1.21e+6 sec
430 psi

@Temperature 167 °F,
Time 336 hour
Overlap
2.99 MPa

@Temperature 75.0 °C,
Time 1.81e+6 sec
433 psi

@Temperature 167 °F,
Time 504 hour
Overlap
4.66 MPa

@Temperature -34.0 °C,
Time 1.81e+6 sec
676 psi

@Temperature -29.2 °F,
Time 504 hour
Overlap
Peel Strength 1.58 kN/m

@Temperature 82.0 °C,
Time 1.81e+6 sec
9.00 pli

@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
1.75 kN/m

@Temperature 24.0 °C,
Time 86400 sec
10.0 pli

@Temperature 75.2 °F,
Time 24.0 hour
180°, Canvas/Steel
2.28 kN/m

@Temperature 24.0 °C,
Time 259000 sec
13.0 pli

@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
2.98 kN/m

@Temperature 24.0 °C,
Time 432000 sec
17.0 pli

@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
3.33 kN/m

@Temperature 24.0 °C,
Time 605000 sec
19.0 pli

@Temperature 75.2 °F,
Time 168 hour
180°, Canvas/Steel
3.86 kN/m

@Temperature 24.0 °C,
Time 1.21e+6 sec
22.0 pli

@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
4.03 kN/m

@Temperature 24.0 °C,
Time 1.81e+6 sec
23.0 pli

@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
4.91 kN/m

@Temperature -34.0 °C,
Time 1.81e+6 sec
28.0 pli

@Temperature -29.2 °F,
Time 504 hour
180°, Canvas/Steel
Thermal Properties Metric English Comments
Flash Point -25.0 °C
-13.0 °F
TCC
Processing Properties Metric English Comments
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Appearance Light Yellow
Base Polychloroprene