Material Notes:
3M™ Scotch-Weld™ Neoprene Contact Adhesive 5 is a sprayable contact adhesive which may be used to bond many high-pressure plastic laminates to wood, particle-board, metal and other surfacesInformation provided by 3M
Physical Properties Metric English Comments
Solids Content 18 - 21 %
18 - 21 %
Brookfield Viscosity 175 - 350 cP
175 - 350 cP
RVF #2 sp @ 20 rpm @ 80°F
Mechanical Properties Metric English Comments
Shear Strength 0.262 MPa

@Temperature 107 °C,
Time 1.81e+6 sec
38.0 psi

@Temperature 225 °F,
Time 504 hour
Overlap
0.448 MPa

@Temperature 82.0 °C,
Time 1.81e+6 sec
65.0 psi

@Temperature 180 °F,
Time 504 hour
Overlap
3.31 MPa

@Temperature 75.0 °C,
Time 1.21e+6 sec
480 psi

@Temperature 167 °F,
Time 336 hour
Overlap
3.32 MPa

@Temperature 75.0 °C,
Time 1.81e+6 sec
482 psi

@Temperature 167 °F,
Time 504 hour
Overlap
7.31 MPa

@Temperature -34.0 °C,
Time 1.81e+6 sec
1060 psi

@Temperature -29.2 °F,
Time 504 hour
Overlap
Peel Strength 1.23 kN/m

@Temperature 82.0 °C,
Time 1.81e+6 sec
7.00 pli

@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
1.75 kN/m

@Temperature 24.0 °C,
Time 86400 sec
10.0 pli

@Temperature 75.2 °F,
Time 24.0 hour
180°, Canvas/Steel
2.10 kN/m

@Temperature 24.0 °C,
Time 259000 sec
12.0 pli

@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
2.45 kN/m

@Temperature 24.0 °C,
Time 432000 sec
14.0 pli

@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
2.89 kN/m

@Temperature -34.0 °C,
Time 1.81e+6 sec
16.5 pli

@Temperature -29.2 °F,
Time 504 hour
180°, Canvas/Steel
3.16 kN/m

@Temperature 24.0 °C,
Time 605000 sec
18.0 pli

@Temperature 75.2 °F,
Time 168 hour
180°, Canvas/Steel
3.16 kN/m

@Temperature 24.0 °C,
Time 1.21e+6 sec
18.0 pli

@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
3.33 kN/m

@Temperature 24.0 °C,
Time 1.81e+6 sec
19.0 pli

@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
Thermal Properties Metric English Comments
Flash Point -25.0 °C
-13.0 °F
TCC
Descriptive Properties Value Comments
Appearance Green, Light Yellow
Base Polychloroprene