Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 295 MPa @Thickness 5.00 - 20.0 mm |
42800 psi @Thickness 0.197 - 0.787 in |
Typical Strength |
Constellium PLAN 5083 Aluminum Rolled Plate Rolled plates in 5083 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5083 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Tensile Strength | 295 MPa @Thickness 20.0 - 150 mm |
42800 psi @Thickness 0.787 - 5.91 in |
Typical Strength |
Constellium PLAN 5083 Aluminum Rolled Plate Rolled plates in 5083 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5083 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Tensile Strength | 295 MPa @Thickness 4.00 - 20.0 mm |
42800 psi @Thickness 0.157 - 0.787 in |
Typical Strength |
Constellium PLAN 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5754 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Tensile Strength | 295 MPa @Thickness 20.0 - 150 mm |
42800 psi @Thickness 0.787 - 5.91 in |
Typical Strength |
Constellium PLAN 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5754 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Tensile Strength | >= 295 MPa @Thickness 12.5 - 60.0 mm |
>= 42800 psi @Thickness 0.492 - 2.36 in |
Temper T651; Standard EN 485-2 |
Constellium PLAN 6082 Aluminum Rolled Plate Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Tensile Strength | >= 295 MPa @Thickness 60.0 - 100 mm |
>= 42800 psi @Thickness 2.36 - 3.94 in |
Temper T651; Standard EN 485-2 |
Constellium PLAN 6082 Aluminum Rolled Plate Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Tensile Strength | 295 MPa @Thickness 4.00 - 20.0 mm |
42800 psi @Thickness 0.157 - 0.787 in |
Typical Strength |
Constellium PLAN OX 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN OX are optimized for minimum residual stress, improved dimensional tolerances and for decorative* anodizing. 5754 PLAN OX is mainly used for low stressed, anodized compone.. |
|||
Tensile Strength | 295 MPa @Thickness 20.0 - 150 mm |
42800 psi @Thickness 0.787 - 5.91 in |
Typical Strength |
Constellium PLAN OX 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN OX are optimized for minimum residual stress, improved dimensional tolerances and for decorative* anodizing. 5754 PLAN OX is mainly used for low stressed, anodized compone.. |
|||
Tensile Strength | 295 MPa @Thickness 8.00 - 20.0 mm |
42800 psi @Thickness 0.315 - 0.787 in |
Typical Strength |
Constellium Planoxal® 50 Aluminum plate Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main.. |
|||
Tensile Strength | 295 MPa @Thickness 20.0 - 100 mm |
42800 psi @Thickness 0.787 - 3.94 in |
Typical Strength |
Constellium Planoxal® 50 Aluminum plate Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main.. |
|||
Tensile Strength | >= 295 MPa @Thickness 12.5 - 60.0 mm |
>= 42800 psi @Thickness 0.492 - 2.36 in |
Temper T651; Standard EN 485-2 |
Constellium Planoxal® 60 Aluminum plate The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly use.. |
|||
Tensile Strength | >= 295 MPa @Thickness 60.0 - 80.0 mm |
>= 42800 psi @Thickness 2.36 - 3.15 in |
Temper T651; Standard EN 485-2 |
Constellium Planoxal® 60 Aluminum plate The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly use.. |
|||
Tensile Strength | >= 295 MPa @Thickness 12.5 - 60.0 mm |
>= 42800 psi @Thickness 0.492 - 2.36 in |
Temper T651; Standard EN 485-2 |
Constellium ALPLAN® 6082 Rolled Precision Aluminum Plate, Milled Both Sides Precision plates in ALPLAN® 6082 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta.. |
|||
Tensile Strength | >= 295 MPa @Thickness 60.0 - 100 mm |
>= 42800 psi @Thickness 2.36 - 3.94 in |
Temper T651; Standard EN 485-2 |
Constellium ALPLAN® 6082 Rolled Precision Aluminum Plate, Milled Both Sides Precision plates in ALPLAN® 6082 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta.. |