Polymer Property : Compressive Modulus = 3210 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 22.1 GPa

@Temperature 177 °C
3210 ksi

@Temperature 351 °F
Hexcel® F161 Epoxy Resin, 7781 Glass Fabric
Hexcel designation: 7781-38"-F161; Fiber: 75-1/0Information provided by HexCel
Compressive Modulus 22.1 GPa

@Temperature 93.0 °C
3210 ksi

@Temperature 199 °F
Hexcel® HexPly® F155 Epoxy Resin, 181 Glass Fabric
Information provided by HexCel
Compressive Modulus 22.1 GPa

@Temperature 24.0 °C
3210 ksi

@Temperature 75.2 °F
Hexcel® HexPly® F155 Epoxy Resin, 220 Glass Fabric
Information provided by HexCel
Compressive Modulus 22.1 GPa

@Temperature 71.0 °C
3210 ksi

@Temperature 160 °F
1/2 hr
Hexcel® HexPly® F515 Epoxy Resin, 1581 Glass Fabric
Hexcel designation: 1581-38"-F515; Fiber 150-1/2Information provided by HexCel